Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.00 MPa | 1160 psi | |
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info.. |