Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 95.1 MPa @Thickness 3.17 mm |
13800 psi @Thickness 0.125 in |
ASTM D638 |
PTS 15GFR-BK PBT- Flame Retardant, 15% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength at Break | 95.1 MPa @Thickness 3.20 mm |
13800 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP2156FM PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength at Break | 95.1 MPa | 13800 psi | ASTM D638 |
PlastxWorld CEVIAN® B6526 30% GF PBT/ABS Alloy Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc. |