Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
Aclo Accutech ABS ABS832G40L Glass Reinforced |
|||
Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
Aclo Accutech SAN SAN930G40L Glass Reinforced |
|||
Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
Aclo Accutech SAN SAN930G30L Glass Reinforced |