Polymer Property : Tensile Strength at Break = 930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.41 MPa

@Temperature 23.0 °C
930 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established...
Tensile Strength at Break 6.41 MPa
930 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength at Break 6.41 MPa

@Temperature 23.0 °C
930 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Strength at Break 6.41 MPa
930 psi
ASTM D412
Teknor Apex Telcar® TL-1050-80 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..