Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 93.8 MPa | 13600 psi | ASTM D638 |
PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength at Break | 93.8 MPa | 13600 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Tensile Strength at Break | 93.8 MPa | 13600 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (DAM)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength at Break | 93.8 MPa | 13600 psi | ASTM D638 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |