Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 93.1 MPa | 13500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
PlastxWorld CEVIAN® B5723 15% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
Chase Plastics CP Pryme® N340HSL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Glass Fiber Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
Chase Plastics CP Pryme® PC320R Polycarbonate, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
Entec Hylox® 9015 PBT, 15% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength at Break | 93.1 MPa | 13500 psi | ASTM D638 |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced