Polymer Property : Tensile Strength at Break = 9.51 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.51 MPa
1380 psi
ASTM D638
LG Chemical LC170 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Tensile Strength at Break 9.51 MPa
1380 psi
DCBP Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..
Tensile Strength at Break 9.51 MPa
1380 psi
DBPH Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..
Tensile Strength at Break 9.51 MPa
1380 psi
Change in tensile strength after 18 hours at 250°F, in vegetable oil; ASTM D471
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..