Polymer Property : Tensile Strength at Break = 9.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.20 MPa
1330 psi
Rate of 50 mm/min; ASTM D 638
NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin
IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Tensile Strength at Break 9.20 MPa
1330 psi
ISO R 527
Stir SpA PVGUM 34 ATC UV (PVC)
Application: Legging boot for dairy useInformation provided by STIR SpA
Tensile Strength at Break 9.20 MPa
1330 psi
ISO 527-1
Barlog Plastics KEBAFLEX SG 85 A.1 TPE-S, Shore A85, natural
TPE-SInformation provided by BARLOG plastics GmbH.
Tensile Strength at Break 9.20 MPa
1330 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,..