Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 61.3 MPa | 8890 psi | ASTM D3759 |
3M 8991 Polyester Tape 3M™ Polyester Tape 8991 is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag sea.. |
|||
Tensile Strength at Break | 61.3 MPa | 8890 psi | ASTM D3759 |
3M 8991L Polyester Tape 3M™ Polyester Tape 8991L is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag se.. |