Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength at Break | 57.9 MPa @Thickness 3.20 mm |
8400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® LW5300M PBT+PC+MF30% Description: Injection Molding, PBT+PC+MF30%, Low WarpageApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 103598-77-2, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength at Break | 57.9 MPa | 8400 psi | ASTM D882 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength at Break | 57.9 MPa | 8400 psi | |
Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLongest pot lifeLarges.. |
|||
Tensile Strength at Break | 57.9 MPa | 8400 psi | |
Abatron AboCast 8103-14 One-Component Epoxy AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting.. |
|||
Tensile Strength at Break | 57.9 MPa | 8400 psi | ASTM D882 |
Spartech APET SP4110 Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |