Polymer Property : Tensile Strength at Break = 8010 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8010 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC)
Information provided by PolyOne
Tensile Strength at Break 55.2 MPa
8010 psi
ASTM D 638
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn..
Tensile Strength at Break 55.2 MPa
8010 psi
ASTM D638
Sumitomo Bakelite North America RX® 3-1-501N-P Mineral Filled Diallyl Phthalate
Mineral filled, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG-F.Information provided by Vyncolit, a Sumitomo Bak Group
Tensile Strength at Break 55.2 MPa
8010 psi
ASTM D638
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate
Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group