Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.829 MPa | 1281 psi | JIS-K-6723 |
Denka LCS Z1050 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |