Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.101 MPa | 1175 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 8.101 MPa | 1175 psi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Tensile Strength at Break | 8.101 MPa | 1175 psi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |