Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.50 MPa | 798 psi | ISO 37 |
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | ISO 37 |
Polyplastic TechnoTep B® 65 A Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Tensile Strength at Break | <= 5.50 MPa | <= 798 psi | ISO/R527 |
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced Information provided by Polykemi AB |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® 3785 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | ISO 37 |
ELASTO UK Dryflex® 3021-001 TPE, Modified Injection Molding Grade for Sanitary Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3021-001 is specifically designe.. |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Tensile Strength at Break | 5.50 MPa | 798 psi | ASTM D638 |
Arkema Group LOTADER® 4700 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4700 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reacti.. |