Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 73.8 MPa | 10700 psi | 2 in/min; ASTM D638 |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 73.8 MPa | 10700 psi | ASTM D638 |
Ravago Manufacturing Americas Echo® RPC30G BK Polypropylene Homopolymer Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago |
|||
Tensile Strength at Break | 73.8 MPa | 10700 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM 407 L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |