Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 6700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced
Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Chesterton ARC S2 Ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli..
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Chesterton MRS S2 Metal Rebuilding System
An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is..
Tensile Strength at Break 46.2 MPa
6700 psi
Abatron AboCast 8103-27 High-Performance Dielectric Epoxy
AboCast 8103-27 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Americas Styrenics EA3400 High Heat Crystal Polystyrene
Product CharacteristicsLess than 300 parts per million residual volatiles with minimal taste and odor transferExcellent clarity and colorGood toughnessFood Contact CompliantTypical ApplicationsCap l..
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved