Polymer Property : Tensile Strength at Break = 66.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.2 MPa
9600 psi
2 in/min; ASTM D638
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding
Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te..
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized
Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical..
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact
Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica..
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
M. Holland Company PC522UR Polycarbonate
High flowHigh impact resistanceGood mold releaseGood UV resistanceApplications: AppliancesProtective coveringsDecorative displaysHousings
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar..
Tensile Strength at Break 66.2 MPa
9600 psi
2 in/min; ASTM D638
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 66.2 MPa
9600 psi
2 in/min; ASTM D638
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products.