Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 80-0800 Crystal Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8005 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Chase Plastics CP Pryme® ASA300 BK General Purpose (Utility) ASA Molding Resin Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 43.4 MPa | 6300 psi | ASTM D638 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |