Polymer Property : Tensile Strength at Break = 6.21 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D638
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System
Information provided by Reltek LLC
Tensile Strength at Break 6.21 MPa
900 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Tensile Strength at Break 6.21 MPa
900 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8291-85PA Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Multibase Multi-Flex® A 6221 E Black TPE Thermoplastic Elastomer
Forms: PelletsInformation provided by Multibase
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP 2104 Thermoplastic Elastomer
Features: Nice Silken Feel Uses: Safety ProductsInformation Provided by Teknor Apex
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-1870-CR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® TL EF-6123 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® TL-1654G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® TL-2597 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® TL-89-P808A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer
Uses: Automotive Applications; Flexible Grips; Gaskets; General Purpose; Industrial Applications; Roof Vents Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injectio..
Tensile Strength at Break 6.21 MPa
900 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow 959S Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber
AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets.
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-2691A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..