Mechanical Properties Metric English Comments
Tensile Strength at Break 41.3 MPa
5990 psi
ASTM D3759
3M 3363 General Purpose Aluminum Foil Tape
40 lb natural kraft paper liner. Good for narrow slit rolls. UL 723 ClassifiedInformation provided by 3M
Tensile Strength at Break 41.3 MPa
5990 psi
ASTM D3759
3M 33806 Premium Performance Aluminum Foil Tape
High temperature acrylic adhesive of 425°FInformation provided by 3M