Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 41.2 MPa @Thickness 2.00 mm |
5980 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 41.2 MPa | 5980 psi | ASTM D3759 |
3M 5491 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |