Polymer Property : Tensile Strength at Break = 5800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 - 40.0 MPa
4350 - 5800 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Tensile Strength at Break 30.0 - 40.0 MPa
4350 - 5800 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Tensile Strength at Break 30.0 - 40.0 MPa
4350 - 5800 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Tensile Strength at Break 30.0 - 40.0 MPa
4350 - 5800 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Tensile Strength at Break 20.0 - 40.0 MPa
2900 - 5800 psi
ASTM 1457-69 T
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Tensile Strength at Break 20.0 - 40.0 MPa

@Thickness 2.00 mm
2900 - 5800 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal..
Tensile Strength at Break 20.0 - 40.0 MPa

@Thickness 2.00 mm
2900 - 5800 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit..
Tensile Strength at Break 34.0 - 40.0 MPa

@Thickness 2.00 mm
4930 - 5800 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM ..
Tensile Strength at Break 30.0 - 40.0 MPa

@Thickness 1.50 mm
4350 - 5800 psi

@Thickness 0.0591 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF)
Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3..
Tensile Strength at Break 34.0 - 40.0 MPa
4930 - 5800 psi
ASTM D638
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Tensile Strength at Break 34.0 - 40.0 MPa
4930 - 5800 psi
ASTM D638
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Tensile Strength at Break 20.0 - 40.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2900 - 5800 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Tensile Strength at Break 20.0 - 40.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2900 - 5800 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Tensile Strength at Break 34.0 - 40.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
4930 - 5800 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.