Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.10 MPa @Temperature 23.0 °C |
740 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Tensile Strength at Break | 5.10 MPa @Time 7200 sec |
740 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-9000 TPE Product Description: StarGrip GP 45-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Tensile Strength at Break | 5.10 MPa | 740 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-70 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Tensile Strength at Break | 5.10 MPa | 740 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 201-55W255 Thermoplastic Vulcanizate Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and cont.. |
|||
Tensile Strength at Break | 5.10 MPa | 740 psi | Die A; ASTM D412 |
3M SJ5300 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 5.10 MPa | 740 psi | Die A; ASTM D412 |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 5.10 MPa | 740 psi | ASTM D412 |
Multibase Multi-Flex® A 6502 MR Natural TPE Thermoplastic Elastomer Forms: PelletsInformation provided by Multibase |