Mechanical Properties Metric English Comments
Tensile Strength at Break 483 MPa

@Temperature 23.0 °C
70000 psi

@Temperature 73.4 °F
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet..
Tensile Strength at Break 483 MPa
70000 psi
Annealed
Special Metals MONEL® 404 Copper-Nickel Alloy
Data provided by California Fine Wire and the manufacturer, Special Metals.
Tensile Strength at Break 483 MPa
70000 psi
Annealed
California Fine Wire Alloy 52 Nickel Iron Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Stress relieved
California Fine Wire Copper, 27% Nickel Clad
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Annealed
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire
All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Annealed
California Fine Wire Manganin 290 Copper, Manganese, and Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Annealed
California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Hard
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 483 MPa
70000 psi
Annealed
California Fine Wire NIFE 5200 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break >= 483 MPa
>= 70000 psi
Carlson 330 Austenitic Alloy
General DescriptionCarlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°..
Tensile Strength at Break >= 483 MPa
>= 70000 psi
Annealed
Carlson C 400 Nickel-Copper Alloy
General DescriptionCarlson Alloy C 400 is a nickel-copper alloy which provides an excellent combination of high strength, ductility, good weldability, and resistance to corrosion over a wide range o..