Polymer Property : Tensile Strength at Break = 4750 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.8 MPa
4750 psi
ASTM D638
Amco Amalloy® B1172 Polymer Alloy
Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials.