Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 4700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products P107-00 Polypropylene Homopolymer, Natural
Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural
Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 32.4 MPa
4700 psi
Indium Corp. Indalloy 153 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
Chase Plastics CP Pryme® NN300STL (COND, 50% RH) Nylon 66 (Utility Grade), Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 32.4 MPa

@Temperature 22.8 °C
4700 psi

@Temperature 73.0 °F
ASTM D638
Ensinger TECAFINE™ PP Polypropylene (PP)
TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical propert..
Tensile Strength at Break 32.4 MPa
4700 psi
vs. steel; 90 s set time
Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
PlastxWorld CEVIAN® A1300 PA/ABS Alloy, Conditioned
Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc.
Tensile Strength at Break 32.4 MPa

@Thickness 2.00 mm
4700 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
Chase Plastics CP Pryme® PPH100-18M Polypropylene Homopolymer, 18 Melt Flow
Information provided by Chase Plastics.
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 32.4 MPa
4700 psi
2 in/min; ASTM D638
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.