Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 31.7 MPa | 4590 psi | ASTM D3759 |
3M Scotch® 234 General Purpose Masking Tape Scotch® General Purpose Masking Tape 234 is designed to be used in medium temperature paint bake operations.Information provided by 3M |