Mechanical Properties Metric English Comments
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow
Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Tensile Strength at Break 43.4 MPa
6300 psi
chs 2 in/min; ASTM D638
Network Polymers NPS 80-0800 Crystal Polystyrene
Description: Injection Molding GradeInformation provided by Network Polymers Inc.
Tensile Strength at Break 43.4 MPa

@Temperature 175 °C
6290 psi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Techmer ES Plastiblend® ABS 8005
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Chase Plastics CP Pryme® ASA300 BK General Purpose (Utility) ASA Molding Resin
Information provided by Chase Plastics.
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC.
Tensile Strength at Break 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength at Break 43.4 MPa

@Temperature 175 °C
6290 psi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..