Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 29.6 MPa | 4290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 33% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength at Break | 29.6 MPa | 4290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |