Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.59 MPa | 4001 psi | chs 2 in/min; ASTM D638 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |