Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 38.5 MPa | 5580 psi | ISO 527 |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Strength at Break | 38.5 MPa | 5580 psi | ASTM D3759 |
3M 433 Premium Performance Aluminum Foil Tape Silicone adhesive for high temperature resistance; MIL-T-47014, FAR 25.853, UL 746C Recognized; smooth easy unwind; clean, straight edges with minimal wrinkling.Information provided by 3M |