Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 - 35.0 MPa
4060 - 5080 psi
ASTM D638
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Tensile Strength at Break 27.0 - 35.0 MPa
3920 - 5080 psi
ASTM D638
Daikin NEOFLON AP-210AS PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D..
Tensile Strength at Break 27.0 - 35.0 MPa
3920 - 5080 psi
ASTM D638
Daikin NEOFLON AP-230ASL PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc...
Tensile Strength at Break 27.0 - 35.0 MPa
3920 - 5080 psi
ASTM D638
Daikin NEOFLON AP-201 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil..
Tensile Strength at Break 27.0 - 35.0 MPa
3920 - 5080 psi
ASTM D638
Daikin NEOFLON AP-210 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided ..
Tensile Strength at Break 27.0 - 35.0 MPa
3920 - 5080 psi
ASTM D638
Daikin NEOFLON AP-230 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries.
Tensile Strength at Break 28.0 - 35.0 MPa
4060 - 5080 psi
5 mm/min.; IS 867-1963
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Tensile Strength at Break 25.0 - 35.0 MPa
3630 - 5080 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Strength at Break 20.0 - 35.0 MPa
2900 - 5080 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Tensile Strength at Break 25.0 - 35.0 MPa
3630 - 5080 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Strength at Break 20.0 - 35.0 MPa
2900 - 5080 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...