Mechanical Properties Metric English Comments
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products M12P250-01 12% Mica Reinforced Polypropylene Copolymer, Black
Applications: Filler panelsHVAC ductsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
chs 2 in/min; ASTM D638
Network Polymers NPP 50-4052
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
2 in/min; ASTM D638
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black
Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D4745
3M Dyneon™ CC174/N Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% fiberglass & 5% natural molybdenum disulfide blended with PTFE.Information provided by Dyneon, A 3M Company
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Ineos N00N-00 Polypropylene Impact Copolymer
Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req..
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Teknor Apex APEX® 3601-95 Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Teknor Apex APEX® 3611-90 Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Teknor Apex APEX® 60001-L Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D412
Teknor Apex Monprene® MP-1885-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D412
Teknor Apex Monprene® MP-1885UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Teknor Apex APEX® 80459 Polyvinyl Chloride, Flexible
Notes: 105°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Plastics Group Polifil® C-40 40% Calcium Carbonate-Reinforced Polypropylene
Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist..
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Chesterton ARC 855 Abrasion Control Liquid
Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by..
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Chesterton ARC S1 General purpose coating
Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink..