Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-101 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
Tensile Strength at Break 19.0 - 22.0 MPa
2760 - 3190 psi
ASTM D638
Daikin NEOFLON NP-3000 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi..