Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.9 MPa
4480 psi
ASTM D3759
3M 5421 Polyethylene Tape
3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M