Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.30 MPa | 479 psi | Across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength at Break | 3.30 MPa | 479 psi | Across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength at Break | 3.30 MPa | 479 psi | ASTM D638 |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Tensile Strength at Break | 3.30 MPa | 479 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Tensile Strength at Break | 3.30 MPa | 479 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® SF 5596 Thermoplastic Elastomer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength at Break | 3.30 MPa | 479 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |