Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.10 MPa | 450 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | |
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | Wet |
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification a.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D412 |
Teknor Apex Monprene® MP 1141 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D412 |
Teknor Apex Uniprene® UN-2598A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A04 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A05 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A10 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2E97C Polyethylene Protective Tape 3M™ Polyethylene Protective Tape 2E97C is a clear co-extruded multi-polymer film coated with a very high-tack acrylic adhesive system designed especially to help provide temporary protection of aut.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2E98C Polyethylene Protective Tape 3M™ Protective Tape is a self-wound clear and printed tapes made from a co-extruded multi-polymer backing coated with a very high-tack acrylic adhesive system to help provide temporary protection o.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2E98P/S2K Polyethylene Protective Tape 3M™ Protective Tape is a self-wound clear and printed tapes made from a co-extruded multi-polymer backing coated with a very high-tack acrylic adhesive system to help provide temporary protection o.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A12 (Clear) Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A87 Co-Extruded Multi-Polymer Protect Tapes 3M™ Co-Extruded Multi-Polymer Protective Tapes have a high-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A88 Co-Extruded Multi-Polymer Protect Tapes 3M™ Co-Extruded Multi-Polymer Protective Tapes have a high-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2E79 (Clear) Co-Extruded Protective Tape 3M™ Co-Extruded Protective Tapes has a very high-tack adhesive system to help provide temporary protection for many automotive carpet applicationsInformation provided by 3M |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2E93-EZ Protective Carpet Tapes 3M™ Protective Carpet Tapes are easy (EZ) unwind tapes made from a co-extruded multi-polymer backing coated with a high-tack acrylic adhesive to help provide temporary protection for carpet and fab.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D412 |
3M 550 Polyurethane Adhesive Sealant Fast Cure 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D412 |
3M 551 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | ASTM D882 |
3M 2A89 Co-Extruded Multi-Polymer Protect Tapes 3M™ Co-Extruded Multi-Polymer Protective Tapes have a high-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Tensile Strength at Break | 3.10 - 3.45 MPa | 450 - 500 psi | ASTM D412 |
Parker Chomerics CHO-FORM 5541 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-55PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9201-45 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tensile Strength at Break | 3.10 MPa | 450 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8291-60B500 Thermoplastic Vulcanizate
(discontinued **) Product Description: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, P.. |