Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok EC1500 Gap Filling CA Adhesive Cyanoacrylate. General purpose, high viscosity adhesive. Ideal for gap filling of porous surfaces. High bond strength, High viscosity, Excellent for gap filling |
|||
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok EC40 General Purpose Ethyl CA Adhesive Cyanoacrylate. General purpose, cures instantly on rubbers, plastics, & many other materials. High Strength, Medium viscosity, Penetrating action |
|||
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok ECGEL Ethyl CA GEL Adhesive Cyanoacrylate. Non-drip thixotropic gel, ideal for maximum gap filling. Non-drip, Excellent on porous surfaces, Allows post-assembly adjustment |
|||
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok ECS Ethyl CA Adhesive Cyanoacrylate. Designed to penetrate by capillary action between pre-assembled components. High Strength, Low viscosity, Penetrating action |
|||
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok PR100 Plastic & Rubber Adhesive Cyanoacrylate. Medium strength plastic & rubber adhesive. For difficult to bond rubber & plastic. High bond strength, Medium viscosity, Fast cure |
|||
Tensile Strength at Break | 20.68 MPa | 2999 psi | |
Ritelok PR1500 Plastic & Rubber Adhesive Cyanoacrylate. Multi-purpose plastic & rubber adhesive. High strength bond & impact resistance. High bond strength, High viscosity, Excellent for gap filling |