Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.62 MPa | 2846 psi | JIS-K-6723 |
Denka REOMER G G5074 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Tensile Strength at Break | 19.62 MPa | 2846 psi | JIS-K-6723 |
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Tensile Strength at Break | 19.62 MPa | 2846 psi | JIS-K-6723 |
Denka VINYKON M556050 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |