Polymer Property : Tensile Strength at Break = 27.59 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.59 MPa
4001 psi
chs 2 in/min; ASTM D638
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.