Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.40 MPa | 2669 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4449D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4449D is a high hardness grade possessing exceptional tensile strength, superior compression.. |
|||
Tensile Strength at Break | 18.40 MPa | 2669 psi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Tensile Strength at Break | 18.40 MPa | 2669 psi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Tensile Strength at Break | 18.40 MPa | 2669 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |