Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPP 50-0151 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | ISO 527-1/-2 |
DSM Arnitel® EB500 50 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | ISO 527-1/-2 |
DSM Arnitel® EB500 Polyether Ester Elastomer (European and Asian Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M6138 High Density Polyethylene ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness... |
|||
Tensile Strength at Break | >= 26.5 MPa | >= 3840 psi | |
Sibur SKS-30 ARKPN 3rd Group Styrene-Butadiene Rubber (SBR) SBR-1502. For use in the tire industry for production of tire thread and other parts for tires, in rubber technical industry for production of a wide assortment of rubber technical articles, and in.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | ISO R 527 |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | ASTM D3759 |
3M 2393 Premium High Temperature Masking Tape 3M™ Masking Tape 2393 is a smooth, heavy duty, mini-crepe, premium high temperature masking tape. It is specifically designed for those applications where easy removal after bake is important. This.. |
|||
Tensile Strength at Break | 26.5 MPa | 3840 psi | ASTM D638 Die C |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |