Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 2540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.5 MPa
2540 psi
ISO R 527
Stir SpA AF 95 HT 105 CZ (PVC)
Application: Extrusion insulation CEI 20-11 type TI3 and YI8Information provided by STIR SpA
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D412
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D412
Teknor Apex Telcar® TL-90-T707E-100 BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 17.5 MPa
2540 psi
ISO 527-1/-2
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 17.5 MPa
2540 psi
ISO 527-1/-2
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 17.5 MPa
2540 psi
ISO 527-2/50
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance ..
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D412
DuPont Performance Polymers Kalrez® 9500 Fluoroelastomer
DuPont™ Kalrez® 9500 perfluoroelastomer parts are a tan product for Deposition, Ash/Strip and Conductor (Poly/Metal) Etch processes. It has been specifically designed for use in applications where..
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D3759
3M Scotch® 218 Fine Line Tape
Scotch® Fine Line Tape 218 is a high-performance film backed tape with low profile and high adhesion to achieve excellent paint liens and for other masking and holding applications.Information prov..
Tensile Strength at Break 17.5 MPa
2540 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2144 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2144 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D3759
3M Scotch® 862 Reinforced Strapping Tape
Scotch® Strapping Tape is reinforced with continuous polypropylene monofilaments. The polypropylene backing provides excellent abrasion, moisture and scuff resistance. The adhesive is specifically ..
Copyright © lookpolymers.com All Rights Reserved