Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.6 MPa | 3420 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90059 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength at Break | 23.6 MPa | 3420 psi | ASTM D638 |
Teknor Apex APEX® 01-A0402C-112 Polyvinyl Chloride, Semi-Rigid Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: TWP Agency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Tensile Strength at Break | 23.6 MPa | 3430 psi | ASTM D3759 |
3M Scotch® 880 Filament Tape Scotch® Filament Tape 880 is a high performance tape reinforced with continuous, polyester yarn filaments that give the tape high tensile strength, high impact resistance and high cut resistance. T.. |
|||
Tensile Strength at Break | 23.6 MPa | 3420 psi | |
3M 484 Electroplating/Anodizing 3M™ Electroplating/Anodizing Tape 484 Tan, vinyl with a rubber adhesive, abrasion resistant, Tape 484 is designed to provide lower adhesion and unwind that Tape 470.Information provided by 3M |
|||
Tensile Strength at Break | 23.6 MPa | 3430 psi | ASTM D3759 |
3M Scotch® 880MSR Filament Tape Scotch® Filament Tape 880MSR is a high performance transparent filament tape reinforced along its length with continuous polyester-yarn filaments, which gives the tape a very high tensile strength... |