Tensile Strength at Break 21.3 MPa

@Treatment Temp. 145 °C,
Time 2100 sec
3090 psi

@Treatment Temp. 293 °F,
Time 0.583 hour
Cure; ASTM D412
Styron Sprintan® SLR 6430 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-6430 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. In relation to solid rubber the grade is extended with 37.5 p..
Tensile Strength at Break 21.3 MPa
3090 psi
ISO 527-1/-2
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 21.3 MPa
3090 psi
ISO 527-1/-2
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 21.3 MPa
3090 psi
ASTM D3759
3M 8401 Polyester Tape
3M™ Polyester Tape 8401 is designed for splicing many release coated papers.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved