Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 204 MPa | 29600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF007SXC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007SXC is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include : Heat Stabilized . |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV007ESS PA 66 (Europe-Africa-Middle East) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific) LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV007ES PA 66 LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Tensile Strength at Break | 204 MPa | 29600 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |