Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.40 MPa | 203 psi | ASTM-F152 |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Tensile Strength at Break | 1.40 MPa | 203 psi | ASTM D412 and ISO 37 |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Tensile Strength at Break | 1.40 MPa | 203 psi | Average |
Daikin POLYFLON PA-5L PTFE Paper Papers made from POLYFLON PTFE papers are manufactured from POLYFLON PTFE fibrous powder, and do not contain any other substances. This paper is soft, elastic, and has very low gas permeability. P.. |
|||
Tensile Strength at Break | 1.40 MPa | 203 psi | ASTM D412 |
3M 755 Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Tensile Strength at Break | 1.40 MPa | 203 psi | ASTM D3759 |
3M 528 Impact Stripping Tape 3M™ Impact Stripping Tape 528 is a thick impact stripping tape used to provide excellent surface protection during plastic media blast (PMB) paint stripping operations.Information provided by 3M |