Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
STN EN ISO 527-2
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized
PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools..
Tensile Strength at Break 200 MPa
29000 psi
ASTM D638
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized
Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Tensile Strength at Break 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66  (Unverified Data**)
Zytel® 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics applications.Information provided by DuPont Performance Polymers
Tensile Strength at Break 200 MPa
29000 psi
ISO 527-1/-2
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
Tensile Strength at Break 200 MPa
29000 psi
ASTM D638
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Tensile Strength at Break 200 MPa
29000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 200 MPa
29000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EC005R PEI
LNP* THERMOCOMP* EC005R is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features include: Mold Release, Electrically Conductive.
Tensile Strength at Break 200 MPa
29000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66
LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare.
Tensile Strength at Break 200 MPa
29000 psi
ISO 527 Type 1A
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Tensile Strength at Break 200 MPa
29000 psi
ISO 527
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Tensile Strength at Break 200 MPa
29000 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65
Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc..
Tensile Strength at Break 200 MPa
29000 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® AG-35 PA66-GF35
Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy ..
Tensile Strength at Break 200 MPa
29000 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-35 S PA6-GF35
Information provided by EMS Grivory
Tensile Strength at Break 200 MPa
29000 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50
Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Tensile Strength at Break 200 MPa
29000 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
Tensile Strength at Break 200 MPa
29000 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following ..
Tensile Strength at Break 200 MPa
29000 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60
Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p..
Tensile Strength at Break 200 MPa
29000 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Tensile Strength at Break 200 MPa
29000 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Tensile Strength at Break 200 MPa
29000 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 200 MPa
29000 psi
ISO 527
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
Tensile Strength at Break 200 MPa
29000 psi
ISO 527
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
Information provided by Eurotec®
Tensile Strength at Break 200 MPa
29000 psi
ASTM D638
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized
Tensile Strength at Break 200 MPa
29000 psi
5 [mm/min]; ISO 527-1/2
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Strength at Break 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..