Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.4741 MPa @Temperature 85.0 °C, Time 605000 sec |
1954.26 psi @Temperature 185 °F, Time 168 hour |
Heat Aging; ISO 188, Method B |
S&E Specialty Polymers TufTech™ SE11-023E PVC Compound Application: Automotive – PVC, black, exterior weatherable, elastomeric, extrusion molding compound.Information provided by S&E Specialty Polymers |