Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.4 MPa | 1940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 1604-xx27FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength at Break | 13.4 MPa @Temperature 23.0 °C |
1940 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Tensile Strength at Break | 13.4 MPa | 1940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2165 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165 is a 65 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2165 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength at Break | 13.4 MPa | 1940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2165G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165G is a 65 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2165G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 13.4 MPa | 1940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90451 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength at Break | 13.4 MPa | 1940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible MD403KB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |